Optogama, UAB (Lithuania): Optical equipment manufacturer
Please contact the import agency Taihei Boeki for details.
AgGaSe₂ crystal

AGSe crystals
AGSe (AgGaSe₂: gallium silver selenide) crystals are negative uniaxial crystals with a wide transmission bandwidth ranging from approximately 0.7 µm to 18 µm, making them high-performance nonlinear optical materials suitable for nonlinear parametric transformations in the mid-infrared region.
It exhibits particularly excellent performance in mid-infrared wavelength conversion using difference frequency generation (DFG), and when combined with synchronously excited optical parametric oscillators (SPOPOs) using femtosecond and picosecond lasers, it is used as a broadband mid-infrared light source.
AGSe has a high figure of merit (Figure of Merit: approximately 70 pm²/V², refractive index n≈2.6), which is about six times higher than that of its related material, AGS. Although its nonlinear coefficients are slightly inferior to GaSe, it has excellent practicality due to its small walk-off and ease of crystal growth and processing (orientation control, thin film coating).
Furthermore, compared to ZGP, while ZGP has a high figure of merit, its transmission bandwidth (approximately 2–12 µm) is limited, whereas AGSe can handle longer wavelengths, making it suitable for constructing broadband mid-infrared light sources.
Main features
- It exhibits excellent optical properties across a wide transmission bandwidth from 0.73 to 18 µm.
- Low light absorption and scattering loss
- Nonlinear characteristics with a high figure of merit (FOM) in the near-infrared to mid-infrared region.
Application example
- Frequency mixing (DFG/SFG) in the mid-infrared region (~approximately 18 µm)
- Second harmonic generation and upconversion for CO₂ lasers
- Tuned wavelength OPO by solid-state laser excitation
Specification.
| Item | Message |
|---|---|
| Orientation accuracy | <30 arcmin |
| Effective opening | >80% |
| External dimensions tolerance | +0.0 / -0.2 mm |
| Parallelism error | <30 arcsec |
| Orthogonality error | <10 arcmin |
| Chamfering | <0.2 mm @45° |
| Surface quality | 60-40 SD |
| coating | BBAR/BBAR @1.7–2.7 µm / 5–18 µm |
| mount | Unimplemented (Unmounted) |
Spectral, thermal, and mechanical properties
| Item | value |
|---|---|
| Chemical formula | AgGaSe₂ |
| Crystal structure | Tetragonal crystal (42m) |
| Lattice constant | a = 5.9920 Å, c = 10.8803 Å |
| optical properties | Negative uniaxial crystal (no > ne, ne > no at λ < 804 nm) |
| density | 5.7 g / cm³ |
| Mohs scale | 3 to 3.5 |
| Transmission wavelength range | 0.71–19 µm |
| Refractive index (@10.5 µm) | no = 2.5917 / ne = 2.5585 |
| Selmeyer formula (no²) | 6.8507 + 0.4297/(λ²−0.1584) − 0.00125λ² |
| Selmeyer formula (ne²) | 6.6792 + 0.4598/(λ²−0.2122) − 0.00126λ² |
| Thermal conductivity (@293 K) | 1.0 W/m·K (∥c) / 1.1 W/m·K (⊥c) |
| Laser damage threshold (LIDT) | >10 MW/cm² @10.6 µm, 150 ns |
technical support
Optogama provides support for selecting AGSe crystals and performing theoretical calculations tailored to your specific application. Please contact us for optimal crystal design advice.
standard product
| Size | Length | θ | φ | coating | Use | Model number |
|---|---|---|---|---|---|---|
| 5 × 5 mm | 2 mm | 52° | 45° | BBAR @1.7–2.7 µm / BBAR @5–18 µm | Ultrashort pulse DFG (1.7–2.7 µm → approx. 5–18 µm, Type I) | 15806 |
| 5 × 5 mm | 5 mm | 52° | 45° | BBAR @1.7–2.7 µm / BBAR @5–18 µm | Ultrashort pulse DFG (1.7–2.7 µm → approx. 5–18 µm, Type I) | 15807 |
| 5 × 5 mm | 10 mm | 52° | 45° | BBAR @1.7–2.7 µm / BBAR @5–18 µm | Ultrashort pulse DFG (1.7–2.7 µm → approx. 5–18 µm, Type I) | 15805 |